Rong Chang 3b0e13173d Debounce charging voltage when cross 8.0V
Link battery pack specification suggested a lower charging current
when voltage pass 8.0V. But the lowering the current in constant
current phase leads voltage drop. And the battery goes back to
high current zone, < 8.0V.

This CL adds a 10 seconds debounce time to prevent charging current
change too quickly.

Signed-off-by: Rong Chang <rongchang@chromium.org>
BUG=chrome-os-partner:9572
TEST=manual
  watch battery V+ on oscilloscope when charging voltage cross 8.0V

Change-Id: I002f941e33b029e38f813ab2e292c6b73a054352
Reviewed-on: https://gerrit.chromium.org/gerrit/27275
Commit-Ready: Rong Chang <rongchang@chromium.org>
Reviewed-by: Rong Chang <rongchang@chromium.org>
Tested-by: Rong Chang <rongchang@chromium.org>
2012-07-15 22:01:14 -07:00
..
2012-07-12 02:35:21 -07:00
2012-07-10 14:56:05 -07:00
2012-07-13 12:24:00 -07:00
2012-07-12 02:35:21 -07:00
2012-06-22 15:35:41 -07:00
2012-06-27 00:55:04 -07:00
2012-06-25 07:15:50 -07:00
2012-05-25 13:34:06 -07:00
2012-06-07 14:33:26 -07:00
2012-05-25 13:34:06 -07:00
2012-07-03 10:50:45 -07:00
2012-06-26 17:01:52 -07:00